A thermal paper manufacturer is printing a company logo on the back of a jumbo thermal paper roll.

The flexographic printing plate is correctly installed, the water-based ink has been prepared, and the paper is moving through the printing unit.

However, the printed logo looks too light.

printed-thermal-paper-jumbo-roll

The operator checks the ink supply and printing pressure, but the problem remains.

Could the anilox roller be responsible?

In flexographic printing, the anilox cell volume controls the amount of ink the roller can hold and helps determine how much ink is delivered to the printing plate.

The cell volume therefore influences the printed image’s colour density, fine detail, drying requirements, and consistency.

For thermal paper printing, this is particularly important because the paper is heat-sensitive and the printed web may enter a slitting and rewinding process shortly afterward.

Too little ink may produce faded logos or incomplete text. Too much ink may cause blurred edges, longer drying requirements, or ink transfer between paper layers.

At JOTA Machinery, we recommend using compatible water-based flexographic ink when printing logos and promotional information on the reverse side of suitable thermal receipt paper.

printing-press-750x563

However, even the correct ink needs an appropriate anilox roller.

This guide explains how anilox cell volume affects thermal paper printing, how to distinguish BCM from LPI, and what manufacturers should consider when selecting an anilox roller for their printing requirements.

1. What Is an Anilox Roller in Flexographic Printing?

An anilox roller is a precision ink-metering component used in flexographic printing.

Its surface contains microscopic engraved cells designed to carry a controlled quantity of ink.

As the anilox roller rotates, ink fills these cells.

A doctor blade or other suitable metering arrangement removes excess ink from the roller surface.

The ink remaining in the cells is then made available for transfer to the raised image areas of the flexographic printing plate.

The printing plate transfers the artwork onto the paper.

How Ink Moves Through the Printing Unit

The process can be divided into four stages.

Ink supply: Water-based flexographic ink is delivered to the anilox roller.

Ink metering: The anilox cells hold a controlled volume of ink while excess ink is removed.

Plate transfer: Ink transfers from the anilox roller to the raised areas of the printing plate.

Paper printing: The printing plate deposits the ink onto the intended paper surface.

The amount of ink ultimately deposited on the thermal paper depends on several factors, including cell volume, cell geometry, ink formulation, doctoring, plate characteristics, impression conditions, and printing speed.

The anilox roller therefore acts as a critical part of the ink-metering system, but it does not determine print results independently.

2. What Does Anilox Cell Volume Mean?

Anilox cell volume describes the total ink-holding capacity of the engraved cells over a defined roller surface area.

It is commonly expressed in BCM, meaning billion cubic microns per square inch.

Another measurement used internationally is cubic centimetres per square metre, written as cm³/m².

These units describe the same physical quantity.

BCM and cm³/m² Conversion

The approximate conversion is:

1 BCM ≈ 1.55 cm³/m²

For example:

Anilox Cell VolumeApproximate Metric Equivalent
1.0 BCM1.55 cm³/m²
2.0 BCM3.10 cm³/m²
3.0 BCM4.65 cm³/m²
4.0 BCM6.20 cm³/m²
5.0 BCM7.75 cm³/m²

These figures describe the engraved cell capacity, not the actual ink volume deposited on the thermal paper.

Only a portion of the ink held in the cells may transfer through the printing system.

The actual amount depends on the entire printing process.

What Happens When Cell Volume Increases?

All else being equal, a higher cell volume can make more ink available for transfer.

This may produce a denser printed image.

However, increasing the volume can also increase the amount of wet ink that must be dried.

For fine artwork, excessive ink can reduce edge definition or cause small image details to merge.

What Happens When Cell Volume Decreases?

A lower cell volume generally makes a smaller quantity of ink available.

This can support finer image reproduction and reduce excessive ink deposition.

However, if the volume is too low for the ink and artwork, solid areas may look weak or fail to achieve the required colour density.

The objective is to select an appropriate ink volume for the actual printing job.

3. How Does Cell Volume Affect Logo Colour Density?

Colour density is one of the most visible effects of anilox selection.

Suppose a customer wants a dark blue company logo printed on the back of a thermal receipt roll.

After printing, the logo appears pale.

The customer expected a stronger colour.

One possible explanation is that the anilox roller is not delivering enough ink for the selected ink formulation and artwork.

When Cell Volume Is Too Low

The printing plate may receive insufficient ink.

Solid areas can appear weak or inconsistent.

Fine text may also become incomplete if ink transfer is inadequate.

However, a light print is not always caused by low anilox volume.

Other possible causes include unsuitable ink viscosity, low pigment strength, clogged anilox cells, inadequate plate contact, or inconsistent ink supply.

The operator should investigate those conditions before replacing the anilox roller.

When Cell Volume Is Too High

Increasing the cell volume can strengthen a solid print under suitable conditions.

But more ink is not always better.

An unnecessarily heavy ink film may cause excessive spreading, reduced edge definition, and increased drying demand.

For thermal paper back printing, the printer must balance adequate colour density with clean artwork reproduction and suitable drying performance.

The correct anilox cell volume is the one that produces the required image using a controlled ink film—not simply the highest available volume.

4. How Does Cell Volume Affect Small Logos and Fine Text?

Many printed thermal receipt rolls contain small graphics.

A retailer may want to print a company logo, website address, promotional message, or terms and conditions on the reverse side.

Some designs include very narrow lines and small lettering.

These details require controlled ink transfer.

Why Excessive Ink Can Reduce Detail

When too much ink is delivered to the printing plate, fine elements may appear thicker than intended.

Small gaps can become partially filled.

Individual dots or adjacent printed features may merge.

This effect is often associated with increased dot gain or image filling.

For a logo containing fine lines, the result may look blurred or less defined.

Can Lower Cell Volume Improve Fine Detail?

An appropriately lower cell volume may reduce excessive ink deposition and improve print sharpness.

However, reducing cell volume too far can produce weak or incomplete images.

The anilox line screen, printing plate, ink formulation, and impression conditions must also be suitable.

Example: Two Different Logo Designs

Consider two printing jobs.

The first involves a large one-colour company logo with broad solid areas.

The second contains a small logo, fine text, and delicate line details.

Although both use water-based flexographic ink, they may require different anilox specifications.

The large solid design may need sufficient ink volume to obtain the approved density.

The detailed design may benefit from a more controlled ink film and a suitable higher cell count.

Anilox selection should therefore begin with the artwork rather than applying the same specification to every job.

5. What Is the Difference Between Anilox BCM and LPI?

Operators sometimes confuse cell volume with anilox line screen.

These specifications are related but measure different characteristics.

BCM measures the ink-holding capacity of the engraved cells per unit surface area.

LPI measures the number of engraved cell lines per linear inch.

A Higher LPI Does Not Automatically Mean More Ink

Higher line-screen values generally indicate a finer cell pattern.

However, the volume depends on cell depth, opening dimensions, engraving geometry, and other characteristics.

Two anilox rollers with the same LPI can have different cell volumes.

Likewise, two rollers with the same BCM value can have different line screens and cell structures.

Why Both Specifications Matter

The line screen influences how the anilox supports fine printing details.

The cell volume influences how much ink is available for transfer.

For high-detail artwork, the selected anilox must provide sufficiently fine ink delivery without losing the required colour density.

For solid artwork, the roller must deliver enough ink while avoiding unnecessarily heavy deposits.

The two specifications should be selected together.

Should You Choose 300 LPI, 400 LPI, or 500 LPI?

There is no universal answer for all thermal paper back-printing applications.

Different artwork, printing plates, water-based inks, and thermal paper grades can require different combinations of line screen and cell volume.

The correct choice should be established with the anilox and ink suppliers using representative printing trials.

Do not select an anilox roller solely because another factory uses the same LPI.

6. How Does Anilox Cell Volume Affect Ink Drying?

Cell volume can influence the quantity of wet ink applied during printing.

That changes the drying demand.

For water-based flexographic ink, drying involves the removal of water and other volatile components from the deposited ink film.

A heavier ink film may require greater drying capacity.

Why Drying Is Important for Thermal Paper

Thermal paper has a heat-sensitive coating.

If the paper experiences unsuitable thermal exposure during the printing process, the coating can develop unwanted background discoloration.

This creates a particular challenge when printing on the reverse side.

The ink needs to dry, but the paper must remain suitable for thermal receipt printing.

What Happens With Excessive Ink Volume?

If the printing system deposits more wet ink than necessary, the dryer may need to remove a greater amount of volatile material.

At a given production speed, the existing drying arrangement may no longer be sufficient.

The result can be incomplete drying or ink transfer during downstream processing.

Why Increasing Dryer Temperature Is Not Always the Solution

Raising the dryer temperature may increase drying capacity, but it can also increase the thermal exposure of the paper.

If the heat-sensitive coating is affected, the product may become unsuitable for its intended application.

Manufacturers should therefore first verify the ink deposit, drying airflow, line speed, and equipment settings.

Choosing an appropriate anilox cell volume can help avoid excessive ink application before drying becomes a problem.

This does not mean that cell volume alone determines drying performance. Ink formulation, airflow, humidity, residence time, and the actual paper temperature also matter.

7. Why Excessive Ink Can Cause Set-Off During Rewinding

After flexographic printing, thermal paper may enter the slitting and rewinding section.

The printed reverse side comes into contact with adjacent layers as the finished rolls are wound.

If the ink film is not sufficiently dry or stable, the printed image may transfer onto another paper surface.

This is known as set-off.

How Anilox Volume Contributes

An unnecessarily high anilox cell volume may increase ink deposition.

If the drying system cannot adequately handle the resulting ink film, the printed paper may reach the rewinding section before it is ready.

The layers are then brought into contact during winding.

Under unsuitable conditions, some ink may transfer from one layer to another.

What Does Set-Off Look Like?

A logo may appear partially duplicated or smeared.

Unwanted ink marks may appear on another surface.

The defect may become more noticeable after the rolls have been stored.

How to Reduce Set-Off

Review the actual ink application level.

Check whether the anilox cell volume suits the artwork and ink.

Verify that the drying process is sufficient at the intended operating speed.

Confirm that the ink is suitable for the specific thermal paper grade.

Conduct winding and storage trials under representative conditions.

Do not assume that a printed sample is ready for rewinding simply because the surface looks dry immediately after printing.

8. Can Low Anilox Cell Volume Cause Printing Defects?

Yes.

Although excessive ink creates its own problems, insufficient ink transfer can also reduce quality.

For example, a thermal receipt paper manufacturer may be printing a solid black logo.

If the anilox system cannot supply enough ink for the required coverage, the logo may appear grey or uneven.

The operator may attempt to correct this by increasing impression pressure.

However, excessive pressure is not an appropriate substitute for insufficient ink delivery.

Check the Cause Before Changing the Anilox

A low-density print may result from:

  • Insufficient anilox cell volume
  • Clogged or worn anilox cells
  • Incorrect ink viscosity or formulation
  • Unsuitable printing plate condition
  • Incorrect impression settings
  • Ink supply or doctoring problems

The operator should determine which factor is responsible.

For example, a roller with an appropriate nominal BCM specification may perform poorly if its cells are heavily contaminated.

Replacing it with a higher-volume roller might hide the immediate symptom without resolving the maintenance problem.

9. Why Anilox Cleaning and Wear Affect Ink Volume

An anilox roller does not necessarily deliver the same ink volume throughout its entire service life.

The engraved cells can accumulate dried ink or other contamination.

The roller surface can also experience wear.

Both conditions can affect the effective ink-carrying capacity.

Clogged Cells

When ink residue occupies part of a cell, the available ink volume decreases.

The roller may deliver less ink even though its original engraved specification has not changed.

A previously acceptable logo may begin printing lighter or less consistently.

Worn Cells

Wear can alter the cell geometry and reduce its effective carrying capacity.

Unlike ordinary ink-supply adjustments, this condition may not be correctable through cleaning.

Why LPI Alone Cannot Reveal Wear

The engraved cell count does not necessarily change as the cells become shallower.

A roller can retain its nominal LPI designation while its effective cell volume decreases.

This is why volume measurement and print-performance records are useful for anilox maintenance.

Cleaning Recommendations

Use the cleaning methods approved by the anilox manufacturer.

Avoid uncontrolled mechanical abrasion or unsuitable chemicals that may damage the engraved surface.

If print density falls unexpectedly, inspect the roller condition before changing the printing plate or increasing pressure.

10. How to Choose the Right Anilox Cell Volume for Thermal Paper

Anilox selection should be based on the full printing application.

For thermal receipt roll back printing, the most important questions concern the artwork, ink, paper, and drying process.

Step 1: Confirm the Artwork

Determine whether the design contains large solid areas, small text, fine lines, or a combination.

The complexity of the artwork influences the required ink-transfer characteristics.

Step 2: Confirm the Ink

JOTA recommends a suitable water-based flexographic ink for thermal paper back printing.

Ask the ink supplier for the recommended anilox specifications for that ink and paper application.

Step 3: Confirm the Thermal Paper Grade

The reverse-side surface may differ between thermal paper products.

These differences can influence ink wetting, adhesion, and print appearance.

Step 4: Review the Available Anilox Rollers

Record each roller’s line screen, cell volume, and relevant engraving details.

Do not compare rollers using LPI alone.

Step 5: Conduct Controlled Printing Trials

Use the approved artwork and representative paper.

Compare print density, fine-detail reproduction, drying behaviour, and overall consistency.

Change one relevant process variable at a time.

Step 6: Evaluate the Finished Rolls

Inspect the printed paper after slitting and rewinding.

Check for set-off, unwanted background marks, and other quality problems.

Test the heat-sensitive side in a compatible receipt printer.

Step 7: Document the Approved Configuration

Record the selected anilox specification, ink grade, printing plate, relevant settings, and inspection results.

This provides a practical reference for future production.

The following observations can help operators identify where to begin.

Printing SymptomPossible Anilox-Related CauseWhat to Check
Logo appears too lightInsufficient effective cell volumeCell cleanliness, wear, BCM and ink transfer
Solid areas are unevenInadequate or inconsistent ink deliveryAnilox condition, ink supply and doctoring
Fine text looks blurredExcessive ink depositionBCM, line screen, plate and impression
Small details fill inExcessive ink transfer or dot gainCell volume and engraving suitability
Ink dries too slowlyInk film may be unnecessarily heavyCell volume, ink and drying capacity
Set-off appears after rewindingIncomplete drying or unstable ink filmInk deposit and drying process
Print density gradually declinesCell contamination or wearCleaning records and measured cell volume
Print varies across the paper widthUneven ink transfer or other press conditionAnilox condition, alignment and doctoring

These are possible causes rather than definitive diagnoses.

For example, fine text may appear blurred because of incorrect plate impression even when the anilox cell volume is appropriate.

Operators should evaluate the complete printing system before deciding that the anilox roller must be replaced.

12. Anilox Cell Volume in Inline Flexo Printing and Slitting

Some thermal paper manufacturers print the reverse-side artwork on a separate flexographic press before slitting and rewinding.

Others use an inline flexographic printing slitter rewinder.

In an integrated arrangement, the unprinted jumbo thermal paper enters the flexographic printing unit first.

The anilox roller supplies ink to the printing plate.

The plate transfers the logo onto the paper.

After appropriate drying, the web proceeds to the slitting and rewinding sections.

Why Ink Control Matters in an Integrated Line

Printing and converting are closely connected.

If the ink film is too heavy, the drying system may limit the sustainable production speed.

If the printed web enters the rewinding section before the ink is sufficiently dry, set-off may occur.

If the cell volume is too low, the finished rolls may contain weak or incomplete logos.

The printing system must therefore produce acceptable artwork while remaining compatible with the downstream converting process.

Printing Speed Is Not the Only Consideration

A machine may have a high rated slitting speed, but the maximum suitable speed for a printed job depends on the printing process and drying conditions.

It should not be assumed that every artwork and ink formulation can be printed at the machine’s maximum mechanical speed.

A production trial should verify the required print quality at the intended operating conditions.

13. JOTA Machinery’s Approach to Thermal Paper Flexographic Printing

At JOTA Machinery, we manufacture thermal paper slitting and rewinding equipment, including configurations with inline flexographic printing.

900A-slitter-rewinder-machine-1125x750

Looking to manufacture custom-printed thermal receipt rolls? The JT-SLT-1400P combines flexographic printing, slitting, and rewinding in one production line. It supports branded POS rolls with logos, advertising messages, and other printed artwork, subject to the printing configuration. For manufacturers planning to add printing capabilities to their converting operations, JOTA can help evaluate the required printing colours, finished roll dimensions, and production specifications.

For back-side logos and promotional artwork, we recommend using a water-based flexographic ink that has been confirmed compatible with the selected thermal paper.

The anilox specification is one of several factors that must be considered when preparing the printing unit.

Why the Artwork Matters

A large one-colour logo and a design containing fine text may not require the same anilox characteristics.

The printing plate, ink formulation, cell volume, and line screen should be reviewed together.

Why Drying Matters

The printed web must reach a suitable drying condition before subsequent converting and winding.

Excessive thermal exposure must be avoided because of the heat-sensitive paper coating.

Why Production Trials Matter

A suitable trial should use the actual thermal jumbo paper grade, intended ink, approved artwork, and representative operating conditions.

The finished rolls can then be inspected for print density, logo clarity, ink adhesion, drying quality, slitting accuracy, and thermal printing performance.

What Information Should Customers Provide?

If you plan to manufacture custom printed thermal receipt rolls, share the thermal jumbo paper grade, finished roll specifications, number of printing colours, artwork, printing repeat requirements, and intended production capacity.

If you already have a preferred water-based ink or anilox specification, provide its technical information as well.

JOTA can review the proposed printing and converting equipment configuration for your application.

The final anilox and ink combination should be confirmed with the relevant suppliers through production testing.

Explore JOTA Thermal Paper Slitting and Inline Flexo Printing Solutions

Conclusion: The Right Anilox Volume Balances Ink Density and Print Quality

Anilox cell volume is one of the main variables affecting ink transfer in thermal paper flexographic printing.

A lower volume can support controlled ink films and fine-image reproduction, but insufficient ink transfer may produce weak printing.

A higher volume can provide more ink for solid areas, but excessive deposition can reduce detail, increase drying demand, and contribute to set-off when the overall process is unsuitable.

The correct selection also depends on anilox line screen, cell geometry, ink formulation, printing plate, thermal paper grade, and machine settings.

For manufacturers using water-based flexographic ink, the objective should be to achieve the required print density and clarity with an ink film that can be dried appropriately before winding.

This is especially important in inline flexographic printing and slitting operations, where the printed web proceeds directly toward finished-roll production.

The best anilox roller is not necessarily the one with the highest BCM or finest LPI. It is the one that consistently delivers the ink required for the approved artwork and thermal paper application.

Planning to Print Logos on Thermal Receipt Rolls?

JOTA Machinery supplies thermal paper slitting and rewinding machines with inline flexographic printing configurations for suitable applications.

If you are establishing a custom printed thermal receipt roll production line or expanding an existing converting operation, our engineering team can review the printing requirements.

Share your paper grade, printing colours, artwork, finished roll dimensions, and production requirements.

We can discuss the appropriate machine configuration and the technical checks needed for a production trial.

Contact JOTA Machinery About Thermal Paper Flexographic Printing